Processes
We are capable of heat treating the processes listed above:
120 | 140 | 170 | 175 | 230 | 250 | 280 | 300 | 340 | Vacuum furnace | |
Max. working T°C | 650° | 950° | 950° | 1150° | 1050° | 1050° | 1050° | 1150° | 1150° | 1700° |
Annealing | X | X | X | X | X | X | X | X | ||
Austenising | X | X | X | X | X | X | ||||
Carburising | X | X | ||||||||
Carbonitriding | X | X | ||||||||
Nitriding | X | X | X | |||||||
Brasing | X | X | X | X | X | X | ||||
Solution annealing | X | X | X | X | X | X | X | X | ||
Debinding / Presintering | X | X | ||||||||
Water quenching | X | X | X | X | X | X | ||||
Salt quenching | X | X | ||||||||
Oil quenching | X | X | X | |||||||
Quenching under high pressure gas | X | X | ||||||||
Furnace forced cooling | X | X | X | X | X | X | X |